Effects of Third-generation LED LCU on Nanomechanical Properties of Orthodontic Adhesives.
In: Acta Physica Polonica: A, Jg. 132 (2017-09-01), Heft 3, S. 697-701
Online
academicJournal
Zugriff:
The aim of this study was to compare the hardness and elastic modulus of orthodontic adhesives cured with different light-curing units, based on light-emitting diodes. Standardized samples of orthodontic adhesives, Transbond XT, Opal® Bond and Light Bond were prepared in cylinder blocks and cured for three seconds with Valo Ortho LED (Ultradent Products, South Jordan, Utah) and Valo LED High-Power Mode. After grinding and polishing, specimens were stored in distilled water at 37 °C for one day. Specimens were investigated using nanoindenter. Employment of Valo Ortho unit has resulted in significantly higher elastic modules for Transbond XT (p = 0:041). The highest nanohardness and elastic modules were measured for Transbond XT cured with Valo Ortho (9.47 GPa; 81.85 GPa, respectively) and lowest for Opal® Bond for both Valo Ortho (0.44 GPa; 14.52 GPa, respectively) and Valo High-Power groups (0.44 GPa; 11.84 GPa, respectively). [ABSTRACT FROM AUTHOR]
Titel: |
Effects of Third-generation LED LCU on Nanomechanical Properties of Orthodontic Adhesives.
|
---|---|
Autor/in / Beteiligte Person: | BILGIC, F. ; ALTAN, H. ; SÖZER, Ö. AKINCI ; ARSLANOGLU, Z. ; KALE, E. ; ÖZARSLAN, S. |
Link: | |
Zeitschrift: | Acta Physica Polonica: A, Jg. 132 (2017-09-01), Heft 3, S. 697-701 |
Veröffentlichung: | 2017 |
Medientyp: | academicJournal |
ISSN: | 0587-4246 (print) |
DOI: | 10.12693/APhysPolA.132.697 |
Schlagwort: |
|