Physical and Morphological Properties of Styrene Butadiene Rubber / Recycled Chloroprene Rubber (SBR/CRr) Blends
In: Advanced Materials Research, Jg. 795 (2013-09-04), Heft 1, S. 119-123
Online
serialPeriodical
Zugriff:
The effects of physical and morphological properties of styrene butadiene rubber/virgin chloroprene rubber blends (SBR/CRv) and styrene butadiene rubber/recycled chloroprene rubber blends (SBR/CRr) were investigated. Both SBR/CRv blends and SBR/CRr blends were prepared using two roll mill at room temperature with blend ratios 95/5, 85/15, 75/25, 65/35 and 50/50. The range size of CRr used in this study was 0.3 0.7 mm. The SBR/CRr blends shows higher value of hardness and crosslink density compared to SBR/CRv blends at all blend ratios. The scanning electron microscopy (SEM) of tensile fracture surface of SBR/CRr blends at 15 blend ratio illustrated a better adhesion and dispersion of CRr with SBR matrix compared with SBR/CRv blends.
Titel: |
Physical and Morphological Properties of Styrene Butadiene Rubber / Recycled Chloroprene Rubber (SBR/CRr) Blends
|
---|---|
Autor/in / Beteiligte Person: | Azrem, Ahmad A. ; Noriman, N.Z. ; Razif, M.N. ; Sam, S.T. ; Saiful Nizwan, M.S. |
Link: | |
Zeitschrift: | Advanced Materials Research, Jg. 795 (2013-09-04), Heft 1, S. 119-123 |
Veröffentlichung: | 2013 |
Medientyp: | serialPeriodical |
ISSN: | 1022-6680 (print) |
DOI: | 10.4028/www.scientific.net/AMR.795.119 |
Sonstiges: |
|